Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 51.4 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 7.00 - 9.00 kN/m
39.9 - 51.4 pli
ASTM D624 Form B
Dow BETAMATE™ 7200 Polyurethane Prepolymer
BETAMATE™ 7200 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It..
Tear Strength 7.00 - 9.00 kN/m
39.9 - 51.4 pli
ASTM D624 Form B
Dow BETAMATE™ 7201 Polyurethane Prepolymer
BETAMATE™ 7201 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It..
Tear Strength 7.00 - 9.00 kN/m
39.9 - 51.4 pli
ASTM D624 Form B
Dow BETAMATE™ 7205 Polyurethane Prepolymer
BETAMATE™ 7205 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It..