Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 50.7 kN/m | 289 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8502 P BLK , 37.5% Filler Content The following data represents the actual data obtained from Lot # 941101-5. The moisture content is 0.03%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 50.7 kN/m | 289 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase SILASTIC® 7-4860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 50.7 kN/m | 289 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 50.7 kN/m | 289 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-560 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 50.7 kN/m | 289 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |