Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 8.50 kN/m | 48.5 pli | ASTM D470 |
DuPont Elvax® 40L-03 Strippable Semiconductive Insulation Shield Formulation
(discontinued **) Elvax® 40L-03 strippable semiconductive insulation shield.Information provided by DuPont. |
|||
Tear Strength | 8.50 kN/m | 48.5 pli | ASTM D470 |
DuPont Elvax® 40L-08 Strippable Semiconductive Insulation Shield Formulation
(discontinued **) Elvax® 40L-08 strippable semiconductive insulation shield.Information provided by DuPont. |