Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 84.0 kN/m | 479 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D 3105 The following is the actual data obtained from the above sample number. This material is based on new generation TPO technology. It has been designed for use as the first shot for airbag covers.Da.. |
|||
Tear Strength | 84.0 kN/m | 479 pli | ISO 34-1B |
Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar.. |