Polymer Property : Tear Strength = 474 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 83.1 kN/m
474 pli
Die C; ASTM D412
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer
Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tear Strength 83.1 kN/m
474 pli
Die C; ASTM D412
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer
Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..