Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 80.0 - 120 kN/m | 456 - 685 pli | Average value: 98.2 kN/m Grade Count:5 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C; ASTM D624 |
Covestro Texin® 5590 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C; ASTM D624 |
Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90010 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 2058A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ISO 34B |
Huntsman AVALON® 80 AE Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1075A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1080A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1085A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1085AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 2080A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene LDPE 2004TC37: Light duty film used for very thin films requiring good optical properties for general packaging.Information provided by Iran Petrochemical Commercial Co. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1285 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1680AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | DIN 53515 |
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C; ASTM D624 |
Covestro Bayflex® 110-35 IMR Polyurethane Elastomeric RIM, 18% Mineral Filled, MDI-based 2-Component Liquid System Calcium Silicate filled. 0.15 in. thickness. IMR=Internal Mold Release RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Ba.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C; ASTM D624 |
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tear Strength | >= 80.0 kN/m | >= 456 pli | ISO 34 |
Austin Novel Materials Texalan® 282A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tear Strength | 80.0 kN/m | 456 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1580 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |