Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 45.1 kN/m | 257 pli | post cured- 8 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4765 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 45.1 kN/m | 257 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tear Strength | 45.1 kN/m | 257 pli | DIN 53515 |
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 70 H 4673 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4673 M is part of the HUNTSMAN injection molding .. |
|||
Tear Strength | 45.1 kN/m | 257 pli | 0.025" extruded film; DIN 53515 |
Huntsman IROGRAN® A 70 H 4714 M TPU-Polyester Introduction: IROGRAN A 70 H 4714 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4714 M is part of the HUNTSMAN injection molding .. |
|||
Tear Strength | 45.1 kN/m | 257 pli | 0.025" extruded film; DIN 53515 |
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
Tear Strength | 45.1 kN/m | 257 pli | Die B,post cured- 2 hours at 177°C; ASTM D624 |
Multibase C6-540 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 45.1 kN/m | 258 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ CF-40 Woven Fabric 550 Information provided by 3M |
|||
Tear Strength | 45.1 kN/m | 258 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ BF-30 Woven Fabric 440 Information provided by 3M |
|||
Tear Strength | 45.1 kN/m | 258 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-62 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 45.1 kN/m | 258 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ BF-40 Woven Fabric 440 Information provided by 3M |
|||
Tear Strength | 45.1 kN/m | 258 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ DF-11 Woven Fabric 610 Information provided by 3M |
|||
Tear Strength | 45.1 kN/m | 258 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ DF-19 Woven Fabric 610 Information provided by 3M |