Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 40.0 - 75.0 kN/m | 228 - 428 pli | Average value: 57.5 kN/m Grade Count:4 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |