Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 40.06 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 40.06 kN/m
228.5 pli
Dow Corning 3730 A&B KIT
A 2 part solventless and colourless liquid silicone rubber with particularly good adhesion to polyamide as well as glass fabric. Cured rubber coating is high strength and has high elongationInformat..