Polymer Property : Tear Strength = 34.6 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 34.6 kN/m
197 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 34.6 kN/m
197 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..