Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 34.4 kN/m | 196 pli | post cured- 4 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4735 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 34.4 kN/m | 196 pli | Die B |
Shin-Etsu Silicones X-30-783U Silicone Elastomer ShinEtsu X30783 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Tear Strength | 34.4 kN/m | 196 pli | Notched, Die B; ASTM D 624 |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 34.4 kN/m | 196 pli | Die C; ASTM D624 |
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer Product Description: Vistamaxx 6102 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Tear Strength | 34.4 kN/m | 196 pli | Die C; ASTM D624 |
ExxonMobil Vistamaxx™ 6102FL Propylene-based Elastomer - Performance Film Product Description: Vistamaxx 6102FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |