Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 33.0 kN/m | 188 pli | ISO 34-1 |
PolyOne OnFlex™ S EF 70A-3S1975 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tear Strength | 33.0 kN/m | 188 pli | ISO 34-1 |
PolyOne OnFlex™ S EH 80A-3S7005 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tear Strength | >= 33.0 kN/m | >= 188 pli | Method B, angle die, 500mm/min.; ISO 34-1 |
S&E Specialty Polymers TufTech™ SE11-023E PVC Compound Application: Automotive – PVC, black, exterior weatherable, elastomeric, extrusion molding compound.Information provided by S&E Specialty Polymers |
|||
Tear Strength | 33.0 kN/m | 188 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 LV Liquid Silicone Rubber - Low Volatile / High Tear This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 33.0 kN/m | 188 pli | Die B |
Momentive Performance Materials FSE7570-D1 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 33.0 kN/m | 188 pli | |
Shin-Etsu Silicones LIMSâ„¢ KEG2001-40A/B Elastomer KEG2001-40 is a very fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enou.. |
|||
Tear Strength | 33.0 kN/m | 188 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7180-1000 TPE Product Description: StarFlex P 7180-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tear Strength | 33.0 kN/m | 188 pli | ASTM D624 |
ELASTO UK Dryflex® 600750S SEBS Based Material, Filled Qualities, 75A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 33.0 kN/m | 188 pli | ASTM D624 |
ELASTO UK Dryflex® 602750S SEBS Based Material, Filled Qualities, 75A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 33.0 kN/m | 188 pli | ASTM D624 |
ELASTO UK Dryflex® 660750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 33.0 kN/m | 188 pli | ASTM D624 |
ELASTO UK Dryflex® 662750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 33.0 kN/m | 188 pli | Die C; ASTM D624 |
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Tear Strength | 33.0 kN/m | 188 pli | Die C; ASTM D624 |
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tear Strength | 33.0 - 81.3 kN/m | 188 - 464 pli | Average value: 49.0 kN/m Grade Count:7 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |