Mechanical Properties Metric English Comments
Tear Strength 57.6 kN/m
329 pli
Die C, 510 mm/min; ASTM D624
PolyOne Elastamax™ HTE 3080 Polyvinyl Chloride + NBR (PVC+NBR)
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a..
Tear Strength 57.6 kN/m
329 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-330 (HAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 57.6 kN/m
329 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 57.6 kN/m
329 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-330 (HAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 57.6 kN/m
329 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..