Polymer Property : Tear Strength = 3140 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 550 kN/m
3140 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 550 kN/m
3140 pli
ASTM D624
GRECO ISOTHANE 3080AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tear Strength 550 kN/m
3140 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 550 kN/m
3140 pli
Graves, MD; ASTM D1004
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc..
Tear Strength 550 kN/m
3140 pli
Graves, TD; ASTM D1004
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc..
Tear Strength 550 kN/m
3140 pli
Graves, MD; ASTM D1004
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista..
Tear Strength 550 kN/m
3140 pli
Graves, TD; ASTM D1004
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista..
Tear Strength 550 kN/m
3140 pli
Graves, MD; ASTM D1004
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film
UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan..
Tear Strength 550 kN/m
3140 pli
Graves, TD; ASTM D1004
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film
UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan..
Tear Strength 550 kN/m
3140 pli
Graves, MD; ASTM D1004
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film
Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,..
Tear Strength 550 kN/m
3140 pli
Graves, TD; ASTM D1004
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film
Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,..
Tear Strength 550 kN/m
3140 pli
Die C; ASTM D412
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..