Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 29.5 kN/m | 168 pli | post cured- 4 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4720 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 29.5 kN/m | 168 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 Molded Golf Grip FormulationNordel® IP 4520 |