Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 50.1 kN/m | 286 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Luperco 130XL Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 50.0 kN/m | 286 pli | B-type, Vulcanized |
KKPC KOSYN 1507H Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 50.0 kN/m | 286 pli | B-type, Vulcanized |
KKPC KOSYN 1502W Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 50.1 kN/m | 286 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLCOAT® DIPP-119 Thermoplastic Polyurethane Elastomer PEARLCOAT® DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this product.. |
|||
Tear Strength | 50.1 kN/m | 286 pli | Nicked; ISO 34-1B |
Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 82AT0 NAT021 is an 82A aromatic polyether-based, non-halogen flame retardant, thermoplastic polyurethane (TPU) compound.Features: Soft, matte finished, good flame retardant proper.. |
|||
Tear Strength | 50.1 kN/m | 286 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Luperco 130XL Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 50.1 kN/m | 286 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Tear Strength | 50.1 kN/m | 286 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |