Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 28.9 kN/m | 165 pli | as molded; Die B |
Multibase SILASTIC® C7-4550 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 28.9 kN/m | 165 pli | ASTM D624 |
PolyOne Versaflex™ OM 6275-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6275-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. New Prod.. |
|||
Tear Strength | 28.9 kN/m | 165 pli | |
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 61 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
Tear Strength | 28.9 kN/m | 165 pli | ASTM D624 |
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Tear Strength | 28.9 kN/m | 165 pli | ASTM D624 |
Huntsman KRYSTALFLEX® PE 429 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tear Strength | 28.9 kN/m | 165 pli | Die C |
Taiwan PU Corporation UR90 Polyester Urethane Rubber UR90 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Tear Strength | 28.9 kN/m | 165 pli | Initial Tear Strength; ASTM D1004-93 |
Saint-Gobain Tygon® SE-200 Inert Tubing Formulation Description: Tygon® SE-200: Without sacrificing the flexibility, glass-like clarity or outstanding bend radius for which Tygon® tubing is known, Tygon® Inert Tubing can handle many applic.. |
|||
Tear Strength | 28.9 kN/m | 165 pli | ASTM D624 |
Teknor Apex Telcar® TL-1269A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tear Strength | 28.9 kN/m | 165 pli | ASTM D624 |
Colorite Polymers Vinylbond 96-1203-40 Compound Description: Vinylbond 96-1203-40 is a flexible vinyl extrusion compound formulated specifically for the window market industry. This particular compound offers excellent bonding characteristics to .. |
|||
Tear Strength | 28.9 kN/m | 165 pli | Split; ASTM D470 |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and .. |
|||
Tear Strength | 28.9 kN/m | 165 pli | Initial Tear Strength |
Saint-Gobain CHR® 2916-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°F .. |
|||
Tear Strength | 28.9 kN/m | 165 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good fluid resistance and physical properties that meet ASTM F 477 for lo.. |