Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 27.15 kN/m | 154.9 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 6900 LC BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |