Polymer Property : Tear Strength = 254 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 44.6 kN/m
254 pli
ISO 34
Multibase TPSiV® 4100-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
Tear Strength 44.6 kN/m
254 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 44.6 kN/m
254 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 44.5 kN/m
254 pli
Die B,post cured- 2 hours at 177°C; ASTM D624
Multibase C6-165 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 44.5 kN/m
254 pli
ASTM D624
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set ..
Tear Strength 44.6 kN/m
254 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 330ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 44.5 kN/m
254 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 44.6 kN/m
254 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 44.6 kN/m
254 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 44.6 kN/m
254 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 44.5 kN/m
254 pli
Fill; Arlon SQA-TMS-026
Arlon 53423R032 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: cured silicone rubber
Tear Strength 44.6 kN/m
254 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 44.6 kN/m
254 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 330ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 44.5 kN/m
254 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..