Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 40.7 kN/m | 232 pli | post cured- 4 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4765 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 40.6 kN/m | 232 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.6 kN/m | 232 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.7 kN/m | 232 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7390-1000 TPE Product Description: StarFlex P 7390-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tear Strength | 40.6 kN/m | 232 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.6 kN/m | 232 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |