Mechanical Properties Metric English Comments
Tear Strength 37.0 kN/m
211 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Zinc Stearate
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 37.0 kN/m
211 pli
Die B
Momentive Performance Materials Addisilâ„¢ 1060 E Industrial Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 37.0 kN/m
211 pli
Die B
Momentive Performance Materials Addisilâ„¢ 2060 E Industrial Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 37.0 kN/m
211 pli
Die B
Momentive Performance Materials Addisilâ„¢ 462 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 37.0 kN/m
211 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LIM 8040 Liquid Silicone Rubber - Self-Bonding
This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur..
Tear Strength 37.0 kN/m
211 pli
Die B
Momentive Performance Materials Addisilâ„¢ 460 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 37.0 kN/m

@Thickness 1.60 mm
211 pli

@Thickness 0.0630 in
ISO 34 (Method A)
SABIC Innovative Plastics ULTEM STM1700 PEI Copolymer
Siltem STM1700 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxici..
Tear Strength 37.0 kN/m
211 pli
Shin-Etsu Silicones LIMSâ„¢ KEG2000-70A/B Elastomer
KEG2000-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Tear Strength 37.0 kN/m

@Thickness 1.60 mm
211 pli

@Thickness 0.0630 in
ISO 34 (Method A)
SABIC Innovative Plastics ULTEM STM1700 PEI Copolymer (Europe-Africa-Middle East)
Siltem STM1700 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxici..
Tear Strength >= 37.0 kN/m
>= 211 pli
Trelleborg Offshore Vikotherm™ 73780 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Tear Strength 37.0 kN/m
211 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Zinc Stearate
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 37.0 kN/m
211 pli
Formulation Example
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..
Tear Strength 37.0 kN/m
211 pli
T.D., Split Tear @ 254 mm/min; ASTM D1938
Eastman Embrace LV Copolyester for Extruded/Cast Film
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo..
Tear Strength 37.0 kN/m
211 pli
ASTM D624
ELASTO UK Dryflex® 500750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Tear Strength 37.0 kN/m
211 pli
ASTM D624
ELASTO UK Dryflex® 502750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Tear Strength 37.0 kN/m
211 pli
ISO 34-B
AlphaGary Evoprene™ Super G 934 SEBS Thermoplastic Elastomer
Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties..
Tear Strength 37.0 kN/m
211 pli
Formulation Example
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..
Tear Strength 37.0 kN/m
211 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 37.0 kN/m
211 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 37.0 - 147 kN/m
211 - 839 pli
Average value: 73.7 kN/m Grade Count:3