Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.9 kN/m | 119 pli | at 25°C |
Daikin DAI-EL G-781 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Tear Strength | 20.9 kN/m | 119 pli | silicone property; ASTM D624 |
Arlon 49283R040 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber |