Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 31.7 kN/m | 181 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 81A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 31.8 kN/m | 181 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 31.7 kN/m | 181 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 31.7 kN/m | 181 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 81A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 31.8 kN/m | 181 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 General Purpose Molding FormulationNordel® IP 4520 |
|||
Tear Strength | 31.7 kN/m | 181 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 Molded Brake Cup FormulationNordel® IP 4640 |
|||
Tear Strength | 31.8 kN/m | 181 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 31.7 kN/m | 181 pli | 31.7 kN/m at 23°C. Value at 100°C is 11.6 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 251-85 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Tear Strength | 31.7 kN/m | 181 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |