Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 25.0 - 30.0 kN/m | 143 - 171 pli | Die B; ASTM 624 |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Tear Strength | 20.0 - 30.0 kN/m | 114 - 171 pli | Die B; ASTM 624 |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Tear Strength | 13.0 - 30.0 kN/m | 74.2 - 171 pli | ASTM D 624 |
API Megol AM DP2154 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 20.0 - 30.0 kN/m | 114 - 171 pli | Die B; ASTM 624 |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Tear Strength | 20.0 - 30.0 kN/m | 114 - 171 pli | Die B; ASTM 624 |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |