Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 29.5 kN/m | 168 pli | post cured- 4 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4720 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 29.4 kN/m | 168 pli | 50mm/min, @ Break; ASTM D624 |
LG Chemical KEYFLEX TO1065A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |
|||
Tear Strength | >= 29.4 kN/m | >= 168 pli | |
Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer 5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It ha.. |
|||
Tear Strength | 29.4 kN/m | 168 pli | ASTM D412 |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Tear Strength | 29.4 kN/m | 168 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Precipitated Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 29.5 kN/m | 168 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 Molded Golf Grip FormulationNordel® IP 4520 |
|||
Tear Strength | 29.4 kN/m | 168 pli | kg/cm²; JIS-K-6301 |
Denka LCS Z6060 Thermoplastic Elastomer, Injection Molding Grade (general) "DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r.. |
|||
Tear Strength | 29.4 kN/m | 168 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Precipitated Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 29.4 kN/m | 168 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-20 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 29.4 kN/m | 168 pli | |
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 62 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
Tear Strength | 29.4 kN/m | 168 pli | 50mm/min, @ Break; ASTM D624 |
LG Chemical KEYFLEX TO1075AR Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |