Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 27.7 kN/m | 158 pli | as molded; Die B |
Multibase SILASTIC® C7-4535 DICUP R Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 27.7 kN/m | 158 pli | ASTM D624 Die B |
Freudenberg Simrit S314 Silicone Elastomer (VMQ) General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol.. |
|||
Tear Strength | 27.7 kN/m | 158 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 35-HR-9 TPE Product Description: StarTUFF TF 35-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 27.7 kN/m | 158 pli | |
Dow Corning SILASTIC® LS 4-9038 FLUOROSILICONE RUBBER 50 Durometer, off-white, uncatalysed, high temperature grade fluorosilicone base.Information provided by Dow Corning |