Mechanical Properties Metric English Comments
Tear Strength 155 kN/m
885 pli
ASTM D624 (Die C)
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer
PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten..
Tear Strength 155 kN/m
884 pli
ASTM D624
Toyobo PELPRENE™ S2001 Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Tear Strength 155 kN/m
884 pli
ASTM D624
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
Tear Strength 155 kN/m
884 pli
ASTM D624
Toyobo PELPRENE™ S2004FS Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.