Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 15.0 kN/m | 85.6 pli | D624 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Tear Strength | 15.0 - 35.0 kN/m | 85.6 - 200 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 5K Polytetrafluoroethylene Coated Kevlar Fabric PTFE coated Kevlar fabric TISOFLON®Information provided by Isoflon. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2735/30 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Karina CAK 65-48/1-F Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Karina E 4048/1-TRE Kariprene Black Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Karina E 5025/1-TRE Kariprene Natural Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials HV 3/506 Heat Cured Rubber - High Temperature Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B473 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B500 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B700 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B800 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg Commercial Neoprene® C653 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg R448 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg Neoprene® C432 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 5029-104 TPE, Modified Injection Molding Grade for Door Stops The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5029-104 is specifically designe.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8014-101 Flame Retardant TPE for Extrusion, Black Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Tear Strength | 15.0 - 55.0 kN/m | 85.6 - 314 pli | Average value: 28.5 kN/m Grade Count:19 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | ISO 4674-1 Method B |
Rogers Corporation Bisco® A2 R 1.5 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tea.. |