Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 148 kN/m | 844 pli | without incision; ISO 34B |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Tear Strength | 148 kN/m | 844 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1495EC Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 148 kN/m | 844 pli | Die C; ASTM D624 |
DuPont™ Surlyn® 8940 Ionomer Resin, Sodium Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |