Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 25.8 kN/m | 147 pli | post cured- 4 hours at 204°C; Die B |
Multibase SILASTIC® C7-4535 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 25.7 kN/m | 147 pli | ASTM D624 |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Tear Strength | 25.7 kN/m | 147 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.7 kN/m | 147 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Die C; ASTM D624C-73 |
3M QI-18/57-325 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Die C; ASTM D624C-73 |
3M QI-5/16-220 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Die C; ASTM D624C-73 |
3M QI-10/37-270 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Die C; ASTM D624C-73 |
3M QSLV-M-2-500 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Die C; ASTM D624C-73 |
3M QSLV-M-8-2/0 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 25.8 kN/m | 147 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |