Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 147 kN/m | 840 pli | ASTM D624 |
Huntsman IROGRAN® A 98 P 4535 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Tear Strength | 147 kN/m | 840 pli | 50mm/min, at Break; ASTM D624 |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Tear Strength | 147 kN/m | 840 pli | 50mm/min, at Break; ASTM D624 |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Tear Strength | 147 kN/m | 840 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® S195A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 147 kN/m | 840 pli | Die C; ASTM D624 |
Lubrizol Estane® S195A Thermoplastic Polyurethane Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Tear Strength | 147 kN/m | 840 pli | ASTM D1004 |
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Informat.. |
|||
Tear Strength | 147 kN/m | 839 pli | ASTM D624 |
Toyobo E1095A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tear Strength | 147 kN/m | 840 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 195A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |