Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 135 kN/m | 770 pli | ASTM D624 |
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Tear Strength | 135 kN/m | 771 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 11H94 Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H94 is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring adequate hardness as well as excellent flow and mech.. |
|||
Tear Strength | 135 kN/m | 770 pli | ASTM D624 |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Tear Strength | 135 kN/m | 770 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-2198 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 135 kN/m | 770 pli | ISO 34 |
Chengdu Polyster H5550B Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ b.. |
|||
Tear Strength | 135 kN/m | 770 pli | unnotched; ASTM D624 (C) |
Arkema Group Pebax® 5533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Tear Strength | 135 kN/m | 771 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | 135 kN/m | 770 pli | ASTM D624 |
BASF Elastollan® 695A15N Polyester Type Polyurethane Elastomer This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes.. |
|||
Tear Strength | 135 kN/m | 771 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly.. |
|||
Tear Strength | 135 kN/m | 770 pli | ASTM D624 |
BASF Elastollan® 695A15 Polyester Type Polyurethane Elastomer This grade contains a hydrolytic stabilizer. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are .. |
|||
Tear Strength | 135 kN/m | 770 pli | ASTM D624 |
BASF Elastollan® M85A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |