Mechanical Properties Metric English Comments
Tear Strength 133 kN/m
759 pli
Network Polymers Softflex® 9000
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tear Strength 133 kN/m
760 pli
ASTM D624
Huntsman IROGRAN® A 95 K 4977 TPU-High Temperature Performance
Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov..
Tear Strength 133 kN/m
759 pli
with incision; ISO 34B
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
Tear Strength 133 kN/m
759 pli
without incision; ISO 34B
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 133 kN/m
759 pli
Die C; ASTM D624
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20..
Tear Strength 133 kN/m
759 pli
Die C; ASTM D624
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.