Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 224 kN/m | 1280 pli | ISO 34B |
Huntsman AVALON® 65 DE Thermoplastic Polyurethane Introduction: AVALON 65 DE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DE is part of the AVALON Perform Range and offers a premium soling material for sports foo.. |
|||
Tear Strength | 224 kN/m | 1280 pli | ISO 34B |
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi.. |
|||
Tear Strength | 225 kN/m | 1280 pli | without incision; ISO 34B |
Lubrizol ESTANE® GP65DE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |