Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 18.1 kN/m | 104 pli | JIS K6301-B |
Stellarchem AB845EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Tear Strength | 18.2 kN/m | 104 pli | ASTM D1004 |
Saint-Gobain Tygon® E-1000 Ultra-Soft Laboratory Tubing Soft and flexible, Tygon® E-1000 Non-DEHP laboratory tubing delivers the same performance in a formulation that contains non-DEHP [Bis (2-ethylhexyl) phthalate] plasticizers. The market demand a.. |
|||
Tear Strength | 18.2 kN/m | 104 pli | |
Dow Corning SILASTIC® 25160 SILICONE RUBBER 60 durometer, peroxide cured, general purpose silicone rubber compoundInformation provided by Dow Corning |