Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 103 kN/m | 590 pli | ASTM D624 |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Tear Strength | 103 kN/m | 590 pli | ASTM D624 |
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tear Strength | 103 kN/m | 590 pli | ASTM D624 |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Tear Strength | 103 kN/m | 588 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Tear Strength | 103 kN/m | 588 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Tear Strength | 103 kN/m | 588 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Tear Strength | 103 kN/m | 588 pli | Die C; ASTM D624 |
Lubrizol Estane® X-590A-2FR Thermoplastic Polyurethane Type: Estane® X-590A-2FR TPU is a Shore 89A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Tear Strength | 103 kN/m | 590 pli | |
Dow Corning SILASTIC® LSR 9791-70 A&B KIT 70 Durometer, 2-part, 1 to 1 mix, translucent, molding grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Tear Strength | 103 kN/m | 588 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers |
|||
Tear Strength | 103 kN/m | 590 pli | ISO 34-1 |
Alliance Polymers Viprene™ P55D-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P55D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 103 kN/m | 590 pli | ISO 34-1 |
Alliance Polymers Viprene™ P55D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P55D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 103 kN/m | 588 pli | ASTM D624 |
Toyobo PELPRENE™ P48U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Tear Strength | 103 kN/m | 588 pli | ASTM D624 |
BASF Elastollan® 685A10 Polyester Type Polyurethane Elastomer This grade contains a hydrolytic stabilizer. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are .. |