Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 10.4 kN/m | 59.3 pli | Method B, angle die, 500mm/min.; ISO 34-1 |
S&E Specialty Polymers TufTechâ„¢ 5501124 Vinyl Application: Replacement for TPV/TPR materials for application requiring an excellent compression set properties, Weatherable, Elastomeric, Extrusion Molding Compound. Targeting for GMP PVC 088.Info.. |
|||
Tear Strength | 10.4 kN/m | 59.4 pli | JIS K6301-B |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |