Mechanical Properties Metric English Comments
Puncture Energy 13.1 - 108 J
9.66 - 79.7 ft-lb
Average value: 36.1 J Grade Count:6
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..