Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 4.29 J | 3.17 ft-lb | Dow Method |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Puncture Energy | 4.29 J | 3.17 ft-lb | ExxonMobil Method |
ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018 CA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018CA have outstanding tensile, puncture resistance and very good sealing properties. These.. |