Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 3.56 J | 2.62 ft-lb | Dow Method |
Dow AFFINITY™ PF 1146G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for high speed packaging applications requiring low seal initiation temperature and good machina.. |