Mechanical Properties Metric English Comments
Puncture Energy 3.39 J
2.50 ft-lb
ExxonMobil
ExxonMobil LL 3105.50 Premium High Strength Film Resin  (discontinued **)
LL 3150.32 is a hexene copolymer LLDPE film resin for blown film. Films produced from this resin have excellent tensile and toughness properties, as well as improved stiffness. Combined with good dr..
Puncture Energy 3.39 J
2.50 ft-lb
ExxonMobil Method
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Puncture Energy 3.39 J
2.50 ft-lb
ExxonMobil Method
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Puncture Energy 3.39 J
2.50 ft-lb
ExxonMobil Method
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Puncture Energy 3.39 J
2.50 ft-lb
Dow Method