Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 2.10 J | 1.55 ft-lb | Low Friction Puncture |
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat.. |
|||
Puncture Energy | 2.10 J | 1.55 ft-lb | ISO 6603-2 |
Lanxess Pocan® T 7331 POS151 000000 PBT + PET, 30% Glass Fiber
(discontinued **) PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Puncture Energy | 2.10 J | 1.55 ft-lb | ISO 6603-2 |
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance |
|||
Puncture Energy | 2.10 J @Temperature -30.0 °C |
1.55 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance |
|||
Puncture Energy | 2.10 J @Temperature -30.0 °C |
1.55 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance |
|||
Puncture Energy | 2.10 J | 1.55 ft-lb | ISO 6603-2 |
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Puncture Energy | 2.10 J | 1.55 ft-lb | ISO 6603-2 |
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
Puncture Energy | 2.10 J @Temperature -30.0 °C |
1.55 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Pocan® B 4239 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Puncture Energy | 2.10 J | 1.55 ft-lb | ISO 6603-2 |
Lanxess Pocan® T 7331 000000 PBT + PET, 30% Glass Fiber PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Puncture Energy | 2.10 J @Load <=66.3 kg, Temperature 23.0 °C |
1.55 ft-lb @Load <=146 lb, Temperature 73.4 °F |
ISO 6603-2 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Puncture Energy | 2.10 J | 1.55 ft-lb | Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 2.10 - 3.50 J | 1.55 - 2.58 ft-lb | Average value: 2.50 J Grade Count:5 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |