Mechanical Properties Metric English Comments
Puncture Energy 2.10 J
1.55 ft-lb
Low Friction Puncture
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin
Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat..
Puncture Energy 2.10 J
1.55 ft-lb
ISO 6603-2
Lanxess Pocan® T 7331 POS151 000000 PBT + PET, 30% Glass Fiber  (discontinued **)
PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized
Puncture Energy 2.10 J
1.55 ft-lb
ISO 6603-2
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance
Puncture Energy 2.10 J

@Temperature -30.0 °C
1.55 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance
Puncture Energy 2.10 J

@Temperature -30.0 °C
1.55 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance
Puncture Energy 2.10 J
1.55 ft-lb
ISO 6603-2
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Puncture Energy 2.10 J
1.55 ft-lb
ISO 6603-2
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding
Puncture Energy 2.10 J

@Temperature -30.0 °C
1.55 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Pocan® B 4239 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Puncture Energy 2.10 J
1.55 ft-lb
ISO 6603-2
Lanxess Pocan® T 7331 000000 PBT + PET, 30% Glass Fiber
PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load
Puncture Energy 2.10 J

@Load <=66.3 kg,
Temperature 23.0 °C
1.55 ft-lb

@Load <=146 lb,
Temperature 73.4 °F
ISO 6603-2
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber
PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS.
Puncture Energy 2.10 J
1.55 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance
Puncture Energy 2.10 - 3.50 J
1.55 - 2.58 ft-lb
Average value: 2.50 J Grade Count:5
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..