Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.76 J | 1.30 ft-lb | Exxon Mobil Method |
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
(discontinued **) Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Puncture Energy | 1.76 - 5.84 J | 1.30 - 4.31 ft-lb | Average value: 4.08 J Grade Count:3 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |