Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.68200 GPa | 98.916 ksi | ASTM D790 |
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |