Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.44 GPa | 934 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL NF2020 PPE+PS (Asia Pacific) |
|||
Flexural Modulus | 6.44 GPa | 934 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR LNP* STAT-KON* OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |