Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 91.4 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.630 GPa
91.4 ksi
ASTM D790
3M Dyneon™ PFA 6525N Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra..
Flexural Modulus 0.630 GPa
91.4 ksi
ASTM D790
LG Chemical LUPOL TE-5005H Thermoplastic Elastomer Alloy, Dimensional Stability
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Flexural Modulus 0.630 GPa
91.4 ksi
ASTM D 790
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Flexural Modulus 0.630 GPa
91.4 ksi
ASTM D 790
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific)
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Flexural Modulus 0.630 GPa
91.4 ksi
ASTM D790
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
Flexural Modulus 0.630 GPa
91.4 ksi
ASTM D790
Asahi Glass Fluon® P-63P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Flexural Modulus 0.630 GPa
91.4 ksi
ASTM D790
Asahi Glass Fluon® P-810UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Flexural Modulus 0.630 - 1.60 GPa
91.4 - 232 ksi
Average value: 1.33 GPa Grade Count:10
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..