Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.24 GPa | 905 ksi | ASTM D790 |
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Flexural Modulus | 6.24 GPa | 905 ksi | ISO Value |
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l.. |
|||
Flexural Modulus | 6.24 GPa | 905 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12 LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 6.24 GPa | 905 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Flexural Modulus | 6.24 GPa | 905 ksi | ISO 178 |
Polyplastics Duranex® CN7015 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 6.24 GPa | 905 ksi | ISO Value |
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista.. |
|||
Flexural Modulus | 6.24 GPa | 905 ksi | ISO Value |
BASF Capron® 8232G HS BK-102 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G HS BK-102 is a pigmented black, heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional.. |