Polymer Property : Flexural Modulus = 9.90 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 9.90 GPa
1440 ksi
STN EN ISO 178
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance
PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved..
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178
Nilit FRIANYL A63 W-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 9.90 GPa
1440 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra..
Flexural Modulus 9.90 GPa
1440 ksi
ASTM D790
LATI LAESTRA G/30-V0CT1 30% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Flexural Modulus 9.90 GPa
1440 ksi
1.3 mm/min; ASTM D790
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced
Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s..
Flexural Modulus 9.90 GPa
1440 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.
Flexural Modulus 9.90 GPa
1440 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f..
Flexural Modulus 9.90 GPa
1440 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable..
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp GF008 PSU
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Asia Pacific)
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East)
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend
LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific)
LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Flexural Modulus 9.90 GPa
1440 ksi
ASTM D790
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Flexural Modulus 9.90 GPa
1440 ksi
ASTM D790
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178-93
Wellman Wellamid® GF33AO99-HRBK 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66
Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman.
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178-93
Wellman Wellamid® MRGF25/15 42H-BKDX9 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced
Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins.
Flexural Modulus 9.90 GPa
1440 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610  (Unverified Data**)
20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers
Flexural Modulus 9.90 GPa
1440 ksi
2 mm/min; ISO 178
Eurostar Starflam UF0033 PPA, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam UF0033 is a Mineral Flame Retardant, Halogen Free and Red Phosphorous Free, Glass Reinforced, Polyphthalamide Injection Molding ResinInformation provided by Eurostar.
Flexural Modulus 9.90 GPa
1440 ksi
ISO Data
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry)
Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6.
Flexural Modulus 9.90 GPa
1440 ksi
ISO Data
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Dry)
Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6.
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178-93
Wellman Wellamid® FRGF1850-N1 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
All information provided by Wellman Engineered Resins.