Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.981 - 9.51 GPa | 142 - 1380 ksi | Average value: 3.93 GPa Grade Count:18 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |